1.2767 steel flats | ||||||||
Chemical Composition(%) | ||||||||
C | Si | Mn | P | S | Cr | Mo | Ni | W |
0.40-0.50 | 0.10-0.40 | 0.15-0.45 | ≤0.030 | ≤0.030 | 1.20-1.50 | 0.15-0.35 | 3.80-4.30 | 0.40-0.60 (OPTIONAL) |
Specialty | ||||||||
1.High toughness of mold steel for oil and gas quenching | ||||||||
2.Good hardenability | ||||||||
3.A small amount of quenching distortion | ||||||||
4.Excellent polishing performance | ||||||||
Use | ||||||||
1.Heavy-duty high toughness pressure dies | ||||||||
2.Required high stress forming dies | ||||||||
3.Heavy cold work tools | ||||||||
4.Shear tools | ||||||||
5.Required high hardness and high toughness plastic mold | ||||||||
Heat Treatment | ||||||||
1.Quench: 840-870°c oil or air cooling | ||||||||
2.Tempering temperature: 160~250 °c | ||||||||
3. Hardness: 56HRC | ||||||||
Melting Process | ||||||||
1. EAF: Electric Furnace+LF+VD(Optional) | ||||||||
2. ESR: Electric Furnace+LF+VD+Eleroslag Remelted(Optional) | ||||||||
UT Class | ||||||||
According to Standard of SEP 1921/84,100% Volume, Level C/c, D/d or E/e | ||||||||
Tolerance on Quantity | ||||||||
+/-10% Per Size | ||||||||