D2 alloy steel round bars | |||||||
Chemical Composition(%) | |||||||
C | Si | Mn | P | S | Cr | Mo | V |
1.50-1.60 | 0.10-0.40 | 0.15-0.45 | ≤0.030 | ≤0.030 | 11.0-12.0 | 0.60-0.80 | 0.90-1.10 |
Specialty | |||||||
High penetration, high rigidity, high endurance, small distortion when quench, possess high rigidity of Cr12*210CrW12,.good tenacity, adapt to tool mould of complicated form. | |||||||
Use | |||||||
1. All kinds of cold stamping mold, cut blade and twisting thread board of high endurance and long life | |||||||
Heat Treatment | |||||||
1. Quench: recommend oil of 980-1040°c\wind(re-preheat~500 °c -850 °c )HRC64-62 | |||||||
2. tempering: eliminate stress, stabilize framework, (180-200 °c )≥2 hours HRC63-62 | |||||||
3.Change of temperature of tempering and HRC rigidity (reference) | |||||||
4.Annealing: 780-800 °c slow cooling | |||||||
Melting Process | |||||||
1. EAF: Electric Furnace+LF+VD(Optional) | |||||||
2. ESR: Electric Furnace+LF+VD+Eleroslag Remelted(Optional) | |||||||
UT Class | |||||||
According to Standard of SEP 1921/84,100% Volume, Level C/c, D/d or E/e | |||||||
Tolerance on Quantity | |||||||
+/-10% Per Size |