Ads by Google
Deformed Rebar
1.Standard: BS4449,HRB335 ,HRB400 ,ASTM A 615, GR460B 2.Dia: 8mm,10mm,12mm,14mm,16mm 3.Usage: for building,etc4.MOQ:25tons
♣ Mechanics Performance According to HRB335
Grade | Technical data of the original chemical composition(%) | |||||
C | Mn | Si | S | P | B | |
HRB335 | ≤0.25 | ≤1.60 | ≤0.80 | ≤0.045 | ≤0.045 | >0.0008 |
Physics capability | ||||||
Yield Strength(N/cm2) | Tensile Strength(N/cm2) | Elongation (%) | ||||
≥335 | ≥490 | ≥16 |
♣ Mechanics Performance According to HRB400
Grade | Technical data of the original chemical composition(%) | |||||
C | Mn | Si | S | P | V | |
HRB400 | ≤0.25 | ≤1.60 | ≤0.80 | ≤0.045 | ≤0.045 | 0.04-0.12 |
Physics capability | ||||||
Yield Strength(N/cm2) | Tensile Strength(N/cm2) | Elongation (%) | ||||
≥400 | ≥570 | ≥14 |