Ads by Google
Technical Index | Material&Processes | ||
Hardness After Hardending&Tempering | HB240~280 | Quality 38CrMoALA | |
Nitrided Hardness | HV950~1000 | ||
Nitrided Case Depth | 0.55~0.7mm | Quality Powder Metallurgy Raw Materials | |
Nitrided Brittleness | Less Than Grade 1 | ||
Surface Roughness | Ra 0.4 | ||
Screw Straightness | 0.015mm | Cold/Thermal Spray Hard Metal Process | |
Surface Chromium-Plating’s Hardness After Nitriding≥900HB | Advanced nitriding Process | ||
Chromium –plating Depth | 0.05~0.10mm | Corrosion & Abrasion Resistance Bimetal Spraying Process | |
Alloy Hardness | HRC55~62 | ||
Alloy Depth | 1.5~2.0mm |
rubber extruder screw