... fiber is produced through adding some functional additive, by plastic melting, extruding, high-ratio stretching and special surface disposal. And shaped ... Polyester Crack Elongation 15-20%Fiber Type Multifilament Flaming point >560 C.Deg. Melting Point(°C) >250°C Density(g/cm3) 1.36 ...