Technical Specification
1 Hardness After Hardending&Tempering : HB240~280
2 Nitrided Hardness : HV900~950
3 Nitrided Case Depth : 0.55~0.7mm
4 Nitrided Brittleness :Less Than Grade 1
5 Surface Roughness :Ra 0.4
6 Surface Chromium-Plating’s Hardness After Nitriding≥900HB
7 Chromium –plating Depth :0.05~0.10mm
8 Material&Processes
9 Quality 38CrMoALA
10 GH3#Steel
11 Quality Powder Metallurgy Raw Materials
12 Cold/Thermal Spray Hard Metal Process
13 Advanced nitriding Process
14 Corrosion & Abrasion Resistance Bimetal Spraying Process