Characteristics:
1.elasticity and appearance of the rubber
2.foggy and shinny surface
3.good feeling of touching and strong elasticity
4.sewing directly and recyclable
Natural report:
PROPERTIES | UNIT | VALUE |
Specific gravity | g/cm³ | 0.93 |
Abrasion resistance | m m³ | 140 |
Tensile strength | kg/cm² | 65.52 |
Tear strength | kg/cm | 20-25 |
Elongation | % | 600 |
Hardness | A | 10-65 |
Flexion | Ciclos | >50,000 |
Operating condition (section temperatures of injection molding machine)
T1=135ºC T2=140ºC T3=145ºC T4=145ºC
Open traces presses:60-70Mpa
Second rolling:30-40Mpa
Third rolling:35Mpa
Feeding presses:110Mpa Back pressure: 20-30Mpa
We can make different hardness or density of TR granules according to customer's need.
TR insole material