UHMW Plastic Scraper for Dyeing Machine: 1. Wear resistant etc 2. ISO certificate 3. MOQ: 300 pcs Scraper for Dyeing Machine

Anyang Ultrahigh Industrial Technical Co., Ltd produces professionally UHMWPE Plastic Scraper for Dyeing Machine. 

 

A. UHMWPE Plastic Scraper for Dyeing Machine description

 UHMWPE material has exceptionally low coefficient of friction offering superb sliding properties and is one of the best plastics for wear/abrasion resistance meanwhile tough and impact resistant even at cryogenic temperatures. As a result, it is definite that UHMW polyethylene is a wonderful engineering plastic that can solve many problems that other engineering plastics cannot.

 

B. Characteristics for UHMWPE Plastic Scraper for Dyeing Machine

1. UHMW exhibits virtually no water absorption

2, Non-Toxic

3. Low coefficient of friction

4. Corrosion resistant

5. Abrasion and impact resistant

6. Wear Resistant

7. Dielectric

8. Weatherproof  

 

C. UHMWPE Application Areas

1. Textile Industry:

2. Chemical Industry:

3. Food Processing Industry:

4. Paper Industry:

5. Material Handling:

6. Farm Implement:

7. Mining & Metals Processing Industries:

8. Transportation:

9. Consumer Products:

10. Waste Water Treatment:

 

D. A parameter table for UHMWPE 

Property

ASTM Test

Units Metric (US)

Typical Values

Specific Gravity

D792

gm/cm°

0.926-0.934

Tensile Strength @ Yield

D638

MPa (PSI)

21 (3100)

Tensile Strength @ Break

D638

MPa (PSI)

48 (7000)

Elongation @ Break

D638

%

350

Young's ("E") Modulus (23°C)

D638

MPa (PSI 105)

690 (1.0)

Young's ("E") Modulus (-269°C)

D638

MPa (PSI 105)

2970 (4.3)

Izod Impact Strength (23°C)

D256(1)

J/m (ft-LBS/in notch)

140 (30)

Izod Impact Strength (-40°C)

D256(1)

J/m (ft-LBS/in notch)

100 (21)

Hardness, Shore "D"

D2240

-

62-66

Abrasion Resistance

(2)

-

100

Water Absorption

D570

%

Nil

Relative Solution Viscosity

D4020

dl/gm

2.3-3.5

Density

 

(lbs./cubic in.)

.034

Scraper for Dyeing Machine

Scraper for Dyeing Machine

Ads by Google

Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECOL Limited and/or its subsidiaries and licensors. All rights reserved.