Product Detail
1.BOPP lamination film:good bonding 2.the brightest in the world 3.Both sides with corona treated 4.SGS Certificate BOPP LAMINATING FILM--HZL

DECRIPTION OF PRODUCTS

Environmentally friendly

It is environmentally friendly,nonhazadous to health and safe to use as no toxic gases or volatile content is emitted.Safety in laminating process as no solvent based adhesive is used.

High function

Compared with other solvent lamination,our film is better in clarity and bonding.Strong ability of absorbing powder.It prevents lamination from being pressed,bubbled and shredded off easily.Matt thermal lamination film is good for spot UV and hot stamping.

Easy handing

It is easy to operate once the required temperature is met and no special technique required.

Efficient and energy-saving

Production cost is reduced substantially as there is no film wastage,mixture of adhesive solvent,and no UV heating lamp is reqired.

Adaptable to different kinds of machines

This film is recommended to be used in dry laminator.Small adjustments need to be made to the machine if the film is used in wet laminator.

Process Parameter

Equipment for laminating film:dry and wet film laminator

Temperature: Normal:85~100°C

Special:100~110  °C

Roller pressure:10~18Mpa

Speed:8~50m/min

Remarks:Special laminations refer to those with thicker ink,solid color,high moisture content and bigger size paper.

Application manual

Adjust roller pressure and temperature according to different types of paper and ink.When using the film for the first time or changing to other sizes,we recommend a small trial volume before going into fully mass lamination.The following situation will affect the quality of the film during lamination.When using metal ink.When the ink contains too much wax,dried oil,adhesive,and silicon additive.etc.When the ink is too thick.When the ink is not completely dry.When the paper contains to much moisture.When there is too much powder.
Product specifications and parameters

SPECIFICATION

hzl-19

gloss

hzl-22

gloss

hzl-23

gloss

hzl-24

gloss

hzl-25

gloss

hzl-27

gloss

hza-23

gloss

hza-25

gloss

hza-27

gloss

THICKNESS(µm)

TOTAL

19

22

23

24

25

27

23

24

27

BASE

11

12

14

15

15

15

14

15

15

EVA

8

10

9

9

10

12

9

10

12

WIDTH

(mm)

360 390 440 540 590 780 880 1080 1320 1400 1600 1880 (or as customers’ request)

LENGTH

(m)

200~3000

PAPER CORE

25.4 mm (1 inch),50.8 mm (2 inch),76 mm (3 inch)

BONDING

LESS THAN 2

TENSILE

STRENGTH

MD:2.4*106 dyne/cm  CD:5.3*106 dyne/cm

  