Ads by Google
Expanded graphite with fiberglass+ inconel wire are suitable for sealing under different media, circumstance, temperature and pressure.
Expanded graphite inconel wire
Main properties | Date |
Carbon content (%) | ≥99 |
Sulphur content (PPM) | ≥1100 |
Chloride content(PPM) | ≥50 |
Ash content (%) | ≥2 |
Graphite yarn with cotton lgnition loss (%) | ≥12(3hours at 450°c) |
Graphite yarn with fiberglass lgnition loss(%) | ≥12(3hours at 650°c) |
Technical date | |
Temperature | -200°c to +600°c |
Pressure | 3-50Mpa |
Velocity | 0-20m/s |
PH rang | 0-14 |