Alnico is hard and brittle. Machining or drilling cannot therefore be accomplished by ordinary methods. Holes are usually cored in at the foundry, and magnets are cast close to final size and then finish machined to closer tolerances.
Temperature Effects
Up to about 1,000 F, changes in magnetization are largely reversible and re-magnetizable, while changes above this are largely structural and not fully reversible or re-magnetizable. Approximately 90% of room temperature magnetization is retained at temperatures of up to 1,000 F.